Distorsion,corrosion,erosion and abrasion mechanisms,concerning the faulty section,of the boiler s secondary superheater were studied by on-site measurements and by samples,cut from the tubes.
分别采取现场实测和割取样2种方法对锅炉二次过热器的
、
蚀、冲刷与磨损等主要
效机
进行了分析,并由此得出预防
效的对策。