The metal reflet glaze samples were prepared with the Huxian wheat-meal-stone accession 0%, 5%, 10% and 15% according to the traditional metal reflet glaze formula and then sintered at 950%.
摘要在光泽
基础上,制作了4组
县麦饭石添量为0%,5%,10%,15%
光泽
试样,在950℃温度环境下烧成。